Good Substitution of LCPP Paraffin PVC Plasticizer
Plasticizer C02
Description
C02 is specially used to replace GB standard chlorinated paraffin because paraffin has high viscosity, dense, low plasticity when used as plasticizer. It has obvious application advantage comparing with chlorinated paraffin.
a. Good color, suitable for various of color or colorless down-stream products.
b. High thermal stability, decomposition temperature is higher than same data of paraffin, resistance to processing, lighter smell.
c. Good plasticizing efficiency, the plasticity is 1.5:1 comparing with paraffin, replace same quantity chlorinated paraffin or 30% main plasticizer of paraffin.
d. Good compatibility with PVC raw material, 100% replace chlorinated paraffin.
e. Competitive price, reduce production cost for down-stream enterprises.
UsageToys
Applications
1. Passed SGS certificate compliance with EU RoHS, REACH, SVHC and BPA regulations.
2. Low Pt-Co, suitable for light color or colorless products.
3. Good stability, high plasticizing efficency, mix with main plasticizer not affect products quality.
4. Children toy products request eco-friendly plasticizer if necessary, B02 or F01 could replace 30-40% main plasticizer.
Specification
Pt-Co | ≤300 |
Acid Value(mgKOH/g ) | ≤0.30 |
Heating decrease volume(125 oC,2 h) | ≤0.50 |
Density g/ml(20 oC) | 1.17-1.20 |
Viscosity(mm2/s) | ≤200 |
Flash point(oC) | >175 |