Introduction of antimony ore processing:
The antimony ore beneficiation methods,should be based on the type of ore,mineral composition,mineral structure and embedded Pot and other physical and chemical properties as the basic conditions to select, you should also consider a price component content and meet the requirements of the antimony metallurgical technology and ultimatelyeconomic and other factors.
Antimony ore beneficiation methods, hand-selected, re-election, heavy media separation, flotation:
Hand-selected:Hand-selected use of antimony ores containing of antimony minerals and gangue in color, luster,shape differences.This method,although the original,and greater labor intensity,but for the antimony ore beneficiation still has a special significance:because the aggregates crystal of the antimony mineral often has bulky monomer crystalline or massive,hand-selected can often get a higher grade blockantimony concentrate,suitable for the technical requirements of the antimony metallurgical plant vertical roaster;
Ore particle size suitable for hand-selected, mostly in between 28 to 150 mm. The most antimony processing plant wide level hand-selected, and only the individual processing plant, such as tin mines north mill grading into narrow level hand-selected. Ore often containing mud, so washing operation is often the staging on hand before the election indispensable. Selected ore after washing and hand-selected, is better than not Jingxi ore direct hand-selected effect.
Gravity concentration:
Heavy media beneficiation
Heavy media beneficiation difficulty is the choice of the weighting agent,media preparation and recovery. A substance that is used as aggravating agent practice: the Grinding Wheel corundum waste (ferrosilicon) is ideal. Magnetic material content of the material 70 to 98%, the chemical composition is mainly silicon and iron, through the concentrator media preparation system pulverized to less than 98% of 74 microns made by weighting agents, so that the density of the medium is kept at 2.65 g / cm 3 or so it is entirely possible,and easy recovery and recycling.
Flotation process is the main antimony ore processing method:
Minerals, most of them are easy floating antimony sulfide mineral flotation ore crystallographic sites. Stibnite often precede lead salts as activators also useful copper salt or a combination of lead salts copper salt, then collector flotation. Common collector for the of butyl xanthate or shale oil mixture Diethyldithiocarbamate foaming agent for the pinitol oil or oil; antimony oxide ore is difficult floated ore.