The low pressure casting lift tube is a key part of low pressure die casting machine. In die casting process, molten aluminum (700-900℃)is sent from riser tube to mold cavity every 3~5 minutes..
Compared with traditional steel lift tube, aluminum titanate becomes the optimum material for riser tubes due to its lower thermal expansion, good thermal shock resistance and nonstick aluminum.
Physical and Chemical Index:
Items |
Datas |
Bulk Density |
3.3-3.5g/cm³ |
Flexural Strength |
30-50Mpa |
Porosity |
<8% |
Thermal-expansion coefficient |
0.5-1.5*10-6℃ |
Heat Conductivity (800℃) |
0.86W/m.K |
Feature:
1,Excellent thermal shock resistance
2,No infiltration with the non-ferrous metal
3,Excellent wear resistance
4,Low thermal-expansion coefficient
5,Long service life
Popular Dimension:
Diameter |
Thickness |
Length |
Φ60、Φ80、Φ100 |
18mm |
<1,150mm |
All goods are made based on customers'drawings.